EVALUATION OF ULTRASHORT CREEP TESTS ON HYDRATING CEMENTITIOUS MATERIALS REQUIRES AN EVALUATION PROTOCOL ACCOUNTING FOR CREEP DURING LOAD APPLICATION
HomeAbstacts & SymposiaEVALUATION OF ULTRASHORT CREEP TESTS ON HYDRATING CEMENTITIOUS MATERIALS REQUIRES AN EVALUATION PROTOCOL ACCOUNTING FOR CREEP DURING LOAD APPLICATION
29 November 2024
EVALUATION OF ULTRASHORT CREEP TESTS ON HYDRATING CEMENTITIOUS MATERIALS REQUIRES AN EVALUATION PROTOCOL ACCOUNTING FOR CREEP DURING LOAD APPLICATION